Rinse treatment after anodizing


The dyeing defects that take place because an acid permeates out from the
microgrooves and the thread grooves of the anodized product are prevented.
And it is a dyeing pretreatment agent that improves the leveling properties
of the dyeing.


special features

  • The spots that take place in the grooves and the microgrooves and the dyeing defects in the shapes of the stars are prevented.
  • The stains and the dyeing defects due to the insufficiency of the water are prevented.
  • The leveling property is improved.
  • The color changes when the dyeing gets small.
  • The colorabilities of the alloys, regarding which the uniform dyeing is difficult, are very much enhanced.

points to be cautious about

  • Because the deposition for a long time causes the deterioration on the surface, you must be cautious.
  • In order to raise the solubility or the stirring effect, it is efficient to carry out the air stirring when dissolving.
  • Although the pH when there is the make-up (50g/l) is around 2.0, because the value of the pH gets changed according to the inflows of the acids, the alkalines, etc., there is a need to adjust the pH regularly.
  • Although the liquid can become brown according to the changes of the elapsed time, there is no influence on the performance.

treatment process



  • STEP.1
    pretreatment

  • STEP.2
    anodizing

  • STEP.3
    Anodic Rinse
    Treatment

  • STEP.4
    dyeing

  • STEP.5
    sealing

  • STEP.6
    rinsing

  • STEP.7
    drying

PRODUCT

Rinse treatment after anodizing

Anodic Rinse Treatment

Rinse treatment after anodizing

The dyeing defects that take place because an acid permeates out from the microgrooves and the thread grooves of the anodized product are prevented. And it is a dyeing pretreatment agent that improves the leveling properties of the dyeing.

special features

  • The spots that take place in the grooves and the microgrooves and the dyeing defects in the shapes of the stars are prevented.
  • The stains and the dyeing defects due to the insufficiency of the water are prevented.
  • The leveling property is improved.
  • The color changes when the dyeing gets small.
  • The colorabilities of the alloys, regarding which the uniform dyeing is difficult, are very much enhanced.

points to be cautious about

  • Because the deposition for a long time causes the deterioration on the surface, you must be cautious.
  • In order to raise the solubility or the stirring effect, it is efficient to carry out the air stirring when dissolving.
  • Although the pH when there is the make-up (50g/l) is around 2.0, because the value of the pH gets changed according to the inflows of the acids, the alkalines, etc., there is a need to adjust the pH regularly.
  • Although the liquid can become brown according to the changes of the elapsed time, there is no influence on the performance.

treatment process

  • STEP.1
    pretreatment
  • STEP.2
    anodizing
  • STEP.3
    Anodic Rinse Treatment
  • STEP.4
    dyeing
  • STEP.5
    sealing
  • STEP.6
    rinsing
  • STEP.7
    drying